Steering: Steering Wheel/handle Bar
THE ZINC PLATING OPERATION PERFORMED ON THE UPPER STEERING COLUMN SHAFT COUPLING BOLT CAUSED HYDROGEN EMBRITTLEMENT AND BREAKAGE OF THE BOLT.
Data updated 14 hours ago
1 known recall on record with NHTSA. Data updated 14 hours ago.
THE ZINC PLATING OPERATION PERFORMED ON THE UPPER STEERING COLUMN SHAFT COUPLING BOLT CAUSED HYDROGEN EMBRITTLEMENT AND BREAKAGE OF THE BOLT.
Source: National Highway Traffic Safety Administration public recall data. This page reports official records and is not legal or repair advice.